Atomic defects in high-k materials affect the performance, reliability, variability, and scaling potential of electronic devices. Their characterization is thus of paramount importance, and methods exploiting electrical measurements are highly demanded. In this work we present a novel method for extracting the defect properties from I-V curve hysteresis measured at low electric field in thick metal-insulator-metal (MIM) stacks. The I-V curve hysteresis allows detecting the defects located near the electrode-insulator interfaces and aligned with the stack Fermi level, and extracting their properties. The defects are profiled cross-correlating the information provided by the low-field current hysteresis and the high-field steady-state current. This technique can be applied to MIM stacks fabricated in Back-End-of-Line for capacitors, embedded memories and thin film transistors.

Extraction of Defects Properties in Dielectric Materials from I-V Curve Hysteresis / Torraca, P. L.; Caruso, F.; Padovani, A.; Spiga, S.; Tallarida, G.; Larcher, L.. - In: IEEE ELECTRON DEVICE LETTERS. - ISSN 0741-3106. - 42:2(2021), pp. 220-223. [10.1109/LED.2020.3048079]

Extraction of Defects Properties in Dielectric Materials from I-V Curve Hysteresis

Torraca P. L.;Padovani A.;Larcher L.
2021

Abstract

Atomic defects in high-k materials affect the performance, reliability, variability, and scaling potential of electronic devices. Their characterization is thus of paramount importance, and methods exploiting electrical measurements are highly demanded. In this work we present a novel method for extracting the defect properties from I-V curve hysteresis measured at low electric field in thick metal-insulator-metal (MIM) stacks. The I-V curve hysteresis allows detecting the defects located near the electrode-insulator interfaces and aligned with the stack Fermi level, and extracting their properties. The defects are profiled cross-correlating the information provided by the low-field current hysteresis and the high-field steady-state current. This technique can be applied to MIM stacks fabricated in Back-End-of-Line for capacitors, embedded memories and thin film transistors.
2021
42
2
220
223
Extraction of Defects Properties in Dielectric Materials from I-V Curve Hysteresis / Torraca, P. L.; Caruso, F.; Padovani, A.; Spiga, S.; Tallarida, G.; Larcher, L.. - In: IEEE ELECTRON DEVICE LETTERS. - ISSN 0741-3106. - 42:2(2021), pp. 220-223. [10.1109/LED.2020.3048079]
Torraca, P. L.; Caruso, F.; Padovani, A.; Spiga, S.; Tallarida, G.; Larcher, L.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

Licenza Creative Commons
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11380/1249299
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 12
  • ???jsp.display-item.citation.isi??? 11
social impact