The degradation of polyethylene terephthalate (PET) fibers in alkaline environments limits their use in strain-hardening cementitious composites (SHCC). Prolonged PET exposure to alkaline environments has a detrimental effect on its mechanical performance, mainly due to the physicochemical transformation caused by alkaline hydrolysis. This study presents a tailored cementitious matrix design containing high amounts of limestone and calcined clay, replacing 75 wt% of Portland cement, to attain and maintain the strain-hardening response of composites incorporating PET fibers as dispersed reinforcement. Analytical and mechanical tests were carried out at different curing ages, ranging from 7 to 60 days, to study the effects of aging on virgin PET fibers, both within the matrix and outside it (in the pore solution). The results showed a pronounced degradation of the PET fibers in the test pore solution at pH 12.5, manifested by a progressive reduction in the load-bearing capacity of the individual fibers with prolonged immersion. Conversely, when the PET fibers were aged in-matrix under laboratory conditions and tested under tension, the performance of the corresponding composites showed resilience to aging, exhibiting reasonable tensile strength and remarkable strain capacities that exceeded 4 %.
Employing limestone and calcined clay for preserving the strain-hardening response of PET fiber-reinforced cementitious composites / Ahmed, A. H.; Signorini, C.; Chikhradze, M.; Liebscher, M.; Butler, M.; Mechtcherine, V.. - In: CONSTRUCTION AND BUILDING MATERIALS. - ISSN 0950-0618. - 438:(2024), pp. 1-17. [10.1016/j.conbuildmat.2024.137166]
Employing limestone and calcined clay for preserving the strain-hardening response of PET fiber-reinforced cementitious composites
Signorini C.Conceptualization
;Liebscher M.Conceptualization
;
2024
Abstract
The degradation of polyethylene terephthalate (PET) fibers in alkaline environments limits their use in strain-hardening cementitious composites (SHCC). Prolonged PET exposure to alkaline environments has a detrimental effect on its mechanical performance, mainly due to the physicochemical transformation caused by alkaline hydrolysis. This study presents a tailored cementitious matrix design containing high amounts of limestone and calcined clay, replacing 75 wt% of Portland cement, to attain and maintain the strain-hardening response of composites incorporating PET fibers as dispersed reinforcement. Analytical and mechanical tests were carried out at different curing ages, ranging from 7 to 60 days, to study the effects of aging on virgin PET fibers, both within the matrix and outside it (in the pore solution). The results showed a pronounced degradation of the PET fibers in the test pore solution at pH 12.5, manifested by a progressive reduction in the load-bearing capacity of the individual fibers with prolonged immersion. Conversely, when the PET fibers were aged in-matrix under laboratory conditions and tested under tension, the performance of the corresponding composites showed resilience to aging, exhibiting reasonable tensile strength and remarkable strain capacities that exceeded 4 %.File | Dimensione | Formato | |
---|---|---|---|
Ahmed-et-al-LC3-PET-final_compressed.pdf
Open access
Tipologia:
Versione pubblicata dall'editore
Dimensione
3.26 MB
Formato
Adobe PDF
|
3.26 MB | Adobe PDF | Visualizza/Apri |
Pubblicazioni consigliate
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris