Sol–gel derived glasses comprised of bioactive materials exhibit a high in vitro response, i.e., the capability to form a hydroxycarbonate apatite (HCA) layer that is claimed to be responsible for the bonding between the glass and the host bone. In this paper, the sol–gel bioactive glass 80% SiO2–15% CaO–5% P2O5(B_BG) was modified by adding the biologically relevant elements cerium, gallium and zinc. Structural characterization of the glasses was performed by 29Si MAS NMR and their in vitro response was investigated by soaking them in simulated body fluid (SBF) for up to 15 days at 37 °C. The HCA formation was monitored by XRD, FTIR, SEM-EDS and ICP measurements. Ce3+, Ga3+, and Zn2+can be classified as “intermediate ions”. However, 29Si NMR revealed that Ce3+ions have a more marked role of “modifier ions” than Ga3+ions, while the behavior of Zn2+lies between those of Ce3+and Ga3+. On the other hand, in spite of the decrease in the in vitro response of B_BG by substitution, the glasses show HCA formation after 15 days of soaking. In addition, an increase in substitution of zinc accelerated the formation of HCA along with the formation of the mixed phase CaZn2(PO4)2·2H2O (scholzite) acting as nucleating agent for HCA. Moreover, the therapeutic effect of optimum Zn released as an ionic dissolution product from Zn-glasses could be beneficial to stimulate osteogenesis.

Structural and in-vitro study of cerium, gallium and zinc containing sol-gel bioactive glasses / Shruti, Shruti; Salinas, A.; Menabue, Ledi; Lusvardi, Gigliola; Malavasi, Gianluca; Ferrara, C.; Mustarelli, P.; Vallet Regi, M.. - In: JOURNAL OF MATERIALS CHEMISTRY. - ISSN 0959-9428. - STAMPA. - 22:27(2012), pp. 13698-13706. [10.1039/c2jm31767b]

Structural and in-vitro study of cerium, gallium and zinc containing sol-gel bioactive glasses

SHRUTI, SHRUTI;MENABUE, Ledi;LUSVARDI, Gigliola;MALAVASI, Gianluca;
2012

Abstract

Sol–gel derived glasses comprised of bioactive materials exhibit a high in vitro response, i.e., the capability to form a hydroxycarbonate apatite (HCA) layer that is claimed to be responsible for the bonding between the glass and the host bone. In this paper, the sol–gel bioactive glass 80% SiO2–15% CaO–5% P2O5(B_BG) was modified by adding the biologically relevant elements cerium, gallium and zinc. Structural characterization of the glasses was performed by 29Si MAS NMR and their in vitro response was investigated by soaking them in simulated body fluid (SBF) for up to 15 days at 37 °C. The HCA formation was monitored by XRD, FTIR, SEM-EDS and ICP measurements. Ce3+, Ga3+, and Zn2+can be classified as “intermediate ions”. However, 29Si NMR revealed that Ce3+ions have a more marked role of “modifier ions” than Ga3+ions, while the behavior of Zn2+lies between those of Ce3+and Ga3+. On the other hand, in spite of the decrease in the in vitro response of B_BG by substitution, the glasses show HCA formation after 15 days of soaking. In addition, an increase in substitution of zinc accelerated the formation of HCA along with the formation of the mixed phase CaZn2(PO4)2·2H2O (scholzite) acting as nucleating agent for HCA. Moreover, the therapeutic effect of optimum Zn released as an ionic dissolution product from Zn-glasses could be beneficial to stimulate osteogenesis.
2012
22
27
13698
13706
Structural and in-vitro study of cerium, gallium and zinc containing sol-gel bioactive glasses / Shruti, Shruti; Salinas, A.; Menabue, Ledi; Lusvardi, Gigliola; Malavasi, Gianluca; Ferrara, C.; Mustarelli, P.; Vallet Regi, M.. - In: JOURNAL OF MATERIALS CHEMISTRY. - ISSN 0959-9428. - STAMPA. - 22:27(2012), pp. 13698-13706. [10.1039/c2jm31767b]
Shruti, Shruti; Salinas, A.; Menabue, Ledi; Lusvardi, Gigliola; Malavasi, Gianluca; Ferrara, C.; Mustarelli, P.; Vallet Regi, M.
File in questo prodotto:
File Dimensione Formato  
C2JM3176-GaZnCe.pdf

Accesso riservato

Tipologia: Versione pubblicata dall'editore
Dimensione 839.14 kB
Formato Adobe PDF
839.14 kB Adobe PDF   Visualizza/Apri   Richiedi una copia
Pubblicazioni consigliate

Licenza Creative Commons
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11380/745982
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 74
  • ???jsp.display-item.citation.isi??? 67
social impact