A technique for lifting off thick film DP 9596 print fired on alumina substrate is reported. The positive phoresist is used as a relif mask. Various applications of the technique are also pointed out.

Technique for lifting off thick film printed on alumina / A., Singh; M., Prudenziati; Morten, Bruno. - In: MICROELECTRONICS RELIABILITY. - ISSN 0026-2714. - STAMPA. - 25:(1985), pp. 619-620.

Technique for lifting off thick film printed on alumina

MORTEN, Bruno
1985

Abstract

A technique for lifting off thick film DP 9596 print fired on alumina substrate is reported. The positive phoresist is used as a relif mask. Various applications of the technique are also pointed out.
1985
25
619
620
Technique for lifting off thick film printed on alumina / A., Singh; M., Prudenziati; Morten, Bruno. - In: MICROELECTRONICS RELIABILITY. - ISSN 0026-2714. - STAMPA. - 25:(1985), pp. 619-620.
A., Singh; M., Prudenziati; Morten, Bruno
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

Licenza Creative Commons
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11380/744135
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 2
  • ???jsp.display-item.citation.isi??? 2
social impact