Failure modes and mechanisms of AlGaN/GaN High Electron Mobility Transistors are reviewed. Data from three DC accelerated tests are presented, which demonstrate a closecorrelation between failure modes and bias point. Maximum degradation was found in “semion” conditions, close to the maximum of hot electron generation which was detected with theaid of electroluminescence measurements. This suggests a contribution of hot-electron effects to device degradation, at least at moderate drain bias (Vds < 30 V). A procedure for the characterization of hot carrier phenomena based on electroluminescence microscopy and spectroscopy is described. At high drain bias (Vds> 30 V - 50 V) new failure mechanisms are triggered, which induce an increase of gate leakage current. The latter is possibly related with the inverse piezoelectric effect leading to defect generation due to strain relaxation, and/or to localized permanent breakdown of the AlGaN barrier layer.Results are compared with literature data throughout the text.

Reliability of GaN high-electron-mobility transistors: state of the art and perspectives / G., Meneghesso; Verzellesi, Giovanni; F., Danesin; F., Rampazzo; F., Zanon; A., Tazzoli; M., Meneghini; E., Zanoni. - In: IEEE TRANSACTIONS ON DEVICE AND MATERIALS RELIABILITY. - ISSN 1530-4388. - STAMPA. - 8:2(2008), pp. 332-343. [10.1109/TDMR.2008.923743]

Reliability of GaN high-electron-mobility transistors: state of the art and perspectives

VERZELLESI, Giovanni;
2008

Abstract

Failure modes and mechanisms of AlGaN/GaN High Electron Mobility Transistors are reviewed. Data from three DC accelerated tests are presented, which demonstrate a closecorrelation between failure modes and bias point. Maximum degradation was found in “semion” conditions, close to the maximum of hot electron generation which was detected with theaid of electroluminescence measurements. This suggests a contribution of hot-electron effects to device degradation, at least at moderate drain bias (Vds < 30 V). A procedure for the characterization of hot carrier phenomena based on electroluminescence microscopy and spectroscopy is described. At high drain bias (Vds> 30 V - 50 V) new failure mechanisms are triggered, which induce an increase of gate leakage current. The latter is possibly related with the inverse piezoelectric effect leading to defect generation due to strain relaxation, and/or to localized permanent breakdown of the AlGaN barrier layer.Results are compared with literature data throughout the text.
2008
8
2
332
343
Reliability of GaN high-electron-mobility transistors: state of the art and perspectives / G., Meneghesso; Verzellesi, Giovanni; F., Danesin; F., Rampazzo; F., Zanon; A., Tazzoli; M., Meneghini; E., Zanoni. - In: IEEE TRANSACTIONS ON DEVICE AND MATERIALS RELIABILITY. - ISSN 1530-4388. - STAMPA. - 8:2(2008), pp. 332-343. [10.1109/TDMR.2008.923743]
G., Meneghesso; Verzellesi, Giovanni; F., Danesin; F., Rampazzo; F., Zanon; A., Tazzoli; M., Meneghini; E., Zanoni
File in questo prodotto:
File Dimensione Formato  
tdmr-ganrel.pdf

Accesso riservato

Tipologia: Versione dell'autore revisionata e accettata per la pubblicazione
Dimensione 1.3 MB
Formato Adobe PDF
1.3 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
Pubblicazioni consigliate

Licenza Creative Commons
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11380/593273
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 560
  • ???jsp.display-item.citation.isi??? 515
social impact