Even though additive manufacturing (AM) techniques have been available since the late 1980s, their application in medicine is still striving to gain full acceptance. For the production of dental implants, the use of AM allows to save time and costs, but also to ensure closer dimensional tolerances and higher repeatability, as compared to traditional manual processes. Among the several AM solutions, Laser Powder Bed Fusion (L-PBF) is the most appropriate for the production of metal prostheses. The target of this paper was to investigate the mechanical and microstructural characteristics of Co-Cr-Mo and Ti-6Al-4V alloys processed by L-PBF, with a specific focus on secondary anisotropy that is usually disregarded in the literature. Tensile specimens were built in the EOSINT-M270 machine, along different orientations perpendicular to the growth direction. Density, hardness, and tensile properties were measured and the results combined with microstructural and fractographic examination. For both alloys, the results provided evidence of high strength and hardness, combined with outstanding elongation and full densification. Extremely fine microstructures were observed, sufficient to account for the good mechanical response. Statistical analysis of the mechanical properties allowed to attest the substantial absence of secondary anisotropy. The result was corroborated by the observations of the microstructures and of the failure modes. Overall, the two alloys proved to be high-performing, in very close agreement with the values reported in the datasheets, independently of the build orientation.

Assay of secondary anisotropy in additively manufactured alloys for dental applications / Bassoli, Elena; Denti, Lucia. - In: MATERIALS. - ISSN 1996-1944. - 11:10(2018), pp. 1-16. [10.3390/ma11101831]

Assay of secondary anisotropy in additively manufactured alloys for dental applications

Bassoli, Elena;Denti, Lucia
2018

Abstract

Even though additive manufacturing (AM) techniques have been available since the late 1980s, their application in medicine is still striving to gain full acceptance. For the production of dental implants, the use of AM allows to save time and costs, but also to ensure closer dimensional tolerances and higher repeatability, as compared to traditional manual processes. Among the several AM solutions, Laser Powder Bed Fusion (L-PBF) is the most appropriate for the production of metal prostheses. The target of this paper was to investigate the mechanical and microstructural characteristics of Co-Cr-Mo and Ti-6Al-4V alloys processed by L-PBF, with a specific focus on secondary anisotropy that is usually disregarded in the literature. Tensile specimens were built in the EOSINT-M270 machine, along different orientations perpendicular to the growth direction. Density, hardness, and tensile properties were measured and the results combined with microstructural and fractographic examination. For both alloys, the results provided evidence of high strength and hardness, combined with outstanding elongation and full densification. Extremely fine microstructures were observed, sufficient to account for the good mechanical response. Statistical analysis of the mechanical properties allowed to attest the substantial absence of secondary anisotropy. The result was corroborated by the observations of the microstructures and of the failure modes. Overall, the two alloys proved to be high-performing, in very close agreement with the values reported in the datasheets, independently of the build orientation.
2018
11
10
1
16
Assay of secondary anisotropy in additively manufactured alloys for dental applications / Bassoli, Elena; Denti, Lucia. - In: MATERIALS. - ISSN 1996-1944. - 11:10(2018), pp. 1-16. [10.3390/ma11101831]
Bassoli, Elena; Denti, Lucia
File in questo prodotto:
File Dimensione Formato  
materials-11-01831.pdf

Open access

Descrizione: manuscript
Tipologia: Versione pubblicata dall'editore
Dimensione 9.59 MB
Formato Adobe PDF
9.59 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

Licenza Creative Commons
I metadati presenti in IRIS UNIMORE sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono rilasciati con licenza Attribuzione 4.0 Internazionale (CC BY 4.0), salvo diversa indicazione.
In caso di violazione di copyright, contattare Supporto Iris

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11380/1168785
Citazioni
  • ???jsp.display-item.citation.pmc??? 3
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 8
social impact